Skip to main content
. Author manuscript; available in PMC: 2016 Apr 20.
Published in final edited form as: ACS Nano. 2016 Mar 10;10(3):3486–3495. doi: 10.1021/acsnano.5b07671

Figure 2.

Figure 2

(A) AFM image of BMEPC-loaded DNA origami complex before irradiation. (B) AFM image of BMEPC-loaded DNA origami complex after irradiation. (C) AGE patterns of the photocleaved triangular-shaped DNA origami influencing corresponding to different BMEPC ratios. (D) AGE patterns of the photocleaved BMEPC-loaded DNA origami influencing corresponding to different durations of irradiation time. (E) One-photon induced fluorescence emission spectra of BMEPC-loaded DNA origami complex after different durations of irradiation time at 405 nm. (Lamp: 365 nm, 8 W. Optical Density: 0.067 W/cm2. Irradiation distance: 1 cm.)