Skip to main content
. 2016 Apr 22;6:24870. doi: 10.1038/srep24870

Figure 6.

Figure 6

SEM images of ZNRs grown with preheating method for (a) 5 mins preheating, (b) 10 mins preheating, (c) 15 mins preheating, (d) Schematics of the erosion and deposition of Zn2+ in the 15 mins preheating method, and (e) Schematics of the ZNRs formation and deposition phenomena in the preheating process.