Table 2.

Hyperelastic and damage material parameters used in the homogeneous uniaxial tensile test example. The fracture energy per unit area is computed as: Inline graphic, where L0 is the localization or characteristic length in the reference configuration [85,86].

parameter value
Ogden material behaviour
μ1 4 kPa
μ2 370 kPa
μ3 −5 kPa
α1 6.4
α2 1.9
α3 −4.2
Inline graphic 1.16 kPa1/2
Gf 20 N cm−1
neo-Hookean material behaviour
μ1 1.5 MPa
α1 2.0
Inline graphic 322.8 kPa1/2
Gf 40 N cm−1