Effect of exposure time and degradation on (a) Wettability of poly(Hydroxyethylacrylate-co-2-nitrobenzyl acrylate (p(HEA-co-2-NBA)). (b) Swelling ratio of P(HEA-co-2-NBA). (c) Elastic modulus of P(HEA-co-2-NBA). (d) Cell concentration in P(HEA-co-2-NBA) with fluorescent imagages of (a) 0, (b) 15, and (c) 90 min exposure times. Reprinted with permission from Ramanan et al. [311]. Copyright 2010 The Royal Chemical Society.