Skip to main content
. 2016 May 3;6:25348. doi: 10.1038/srep25348

Figure 3.

Figure 3

(a) Schematic illustration of the microfabrication process of the stretchable Fresnel lens (not to scale); (b) Fabricated device containing 2 × 2 lens units (f = 7 mm), with each unit size 6 × 6 mm2; (c) Optical microscope image of one lens; (d) Tilted SEM image of the diffractive CNT pattern, the inset shows a close up view of the vertically aligned CNT which are 10 μm in height (before PDMS percolation); (e) SEM image of the CNT with the PDMS percolated thoroughly into the CNT bundles; (f) The measured transmittance of the transparent PDMS area and the opaque CNT/PDMS area, with glass as reference. The PDMS has a transmittance of 93.9%, higher than glass (91.8%), while the CNT/PDMS has transmittance of 0.06%.