Skip to main content
. 2015 Sep;12(9):686–694.

Table 1.

The mean shear bond strength values and standard deviations (SD) of groups

Groups Non thermocycled Thermocycled and stored for 6 months
Control 23.35± 3.12 1.80± 1.23
Nd:YAG laser 18.95± 3.46 4.77± 1.72 A
CO2 laser 14.00± 1.96 3.70± 1.56 A

N=15 and all groups were significantly different by Tukey’s test, except the groups with the same superscripted letters (Adjusted P>0.02)