Skip to main content
. 2016 May 5;6:25059. doi: 10.1038/srep25059

Figure 7. Three point bending test of thin bricks self-healing glass/polymer composites.

Figure 7

On the left, optical images of bending before (top) during (middle) and after (bottom) fracture. The bottom picture shows how the composite autonomously reaches the initial configuration and undergoes self-healing at the interfaces The capillary bridges are able to bring the bricks together and reform the structure upon releasing the force and without applying external pressure. On the right, force vs. displacement healing curves of brick/mortar composite samples after set amount of times.