Fig. 6.

Fig. 6

(a) The fractional double-bond conversion measured at 30 min after irradiation as a function of filler content under various instrumental compliances. (b) The real-time evolution of the conversion for selected composites under a compliance of 2.65 μm/N and the corresponding conversion rate during the first 20 s after photo-activation (inset). (c) The real-time evolution of the temperature change (compared to the room temperature) for selected composites. Error bars indicate the standard deviation of the measurement. Data values of the final conversion and maximum temperature rise are given in the SD, Table S3.