Fig. 5.

Fig. 5

DSC thermogram of a CL-EMIm aerogel soaked in o-xylene—the crystallization curve (3) acquired after heating from −70 to −25 °C (2) was used to calculate the PSD. Inset selection of 11 thermograms measured on CL-EMIm aerogels, amplified in the exothermic peak (3) associated with the crystallization of the confined solvent