Table 3. Production of DV230-Ficoll Using Different PEG Length SM-PEGn heterobifunctional linkers.
attribute | DV230-Ficoll conjugates | |||
---|---|---|---|---|
# PEG units in SM-PEGn linker | 6 | 24 | 45 | 70 |
Maleimide:Ficoll molar ratio | 215 | 199 | 227 | 225 |
DV230:Ficoll molar ratio | 109 | 116 | 110 | 108 |
Particle sizea (diameter) by DLS | 55 nm | 77 nm | 78 nm | 91 nm |
Mean particle diameter (nm) values based on intensity distribution measurements.