Skip to main content
. 2016 May 26;6:26462. doi: 10.1038/srep26462

Figure 2.

Figure 2

(a) R/RF data for DPTAP monolayers spread on water subphase Inline graphic, subphase containing AuNPs (10 nm in nominal diameter) of bare surface (Δ), AuNPs (10 nm in nominal diameter) coated with DNA Inline graphic and in the presence of 0.1 M NaCl Inline graphic. The R/RF ≈ 1 at Qz < 0.0218 Å−1 and the data are shifted vertically for clarity. Solid lines are best-fit calculated reflectivities based on the refined parameters. (b) The corresponding electron density profiles across the air-water interface based on the best-fit structural parameters.