Skip to main content
. 2016 Apr 8;3(3):159–166. doi: 10.1093/rb/rbw017

Figure 2.

Figure 2.

Weight loss ratio of P, PR, PT and PRT scaffolds degraded in vitro. (P: poly(d,l-lactic acid); PR: poly(d,l-lactic acid)/RGD peptide modification of poly{(lactic acid)-co-[(glycolic acid) -alt-(L-lysine)]}; PT: poly(d,l-lactic acid)/β-tricalcium phosphate; PRT: poly(d,l-lactic acid)/RGD peptide modification of poly{(lactic acid)-co-[(glycolic acid) -alt-(l-lysine)]}/β-tricalcium phosphate).