Skip to main content
. 2016 May 27;6:26736. doi: 10.1038/srep26736

Figure 2.

Figure 2

Morphology of the (a) ZnAc-PVP nanofibers, (b) ZnO-Fs formed by oxidation of (a) at 500 °C, (c) ZnO-H structure fabricated by hydrothermal method using ZnO-Fs in (b) as seed template, and (d) ZnO/CuO-H structure formed by decoration of CuO nanoparticles on structure in (c). Inset images in (a,b,d) show high magnification SEM. Inset image in (c) shows cross-section view.