Skip to main content
. 2014 Oct 29;2014:702396. doi: 10.1155/2014/702396

Figure 3.

Figure 3

UV-Vis absorbance of silver nanoparticles solutions by time, using 1 mmole/L AgNO3 with 20 g/L NaOH at 60°C. (a) 1 g/L starch, (b) 3 g/L starch, and (c) 6 g/L starch. (d) UV-Vis absorbance of silver nanoparticles solutions by using different concentrations of maize starch, using 1 mmole/L AgNO3 with 20 g/L NaOH at 60°C for 60 minutes.