Skip to main content
. 2016 Jul 13;374(2071):20150279. doi: 10.1098/rsta.2015.0279

Figure 12.

Figure 12.

Normalized compressive strength of different composite laminates depending on void content [2,3,4]. Measurement data: Gehrig (CFRP) are mean values, whereas Bazhenov (GFRP) also investigated the influence of fibre diameter: Inline graphic (black triangle), 80 μm (dark grey triangle) and 130 μm (light grey triangle).