Skip to main content
. 2016 Jun 15;6:27884. doi: 10.1038/srep27884

Figure 7. The diameters of the craters formed on PLGA films.

Figure 7

The time represents immersion time after craters formation. Black closed squares (▪), red triangles (▴), blue closed circles (⦁) indicate the diameters of the crater formed by mechanically milling, the laser ablation craters with 800 nm, 1.0 J/cm2, 15000 pulses, the laser ablation craters with 400 nm, 0.15 J/cm2, 15000 pulses, respectively. All values are expressed as means ± standard deviation (SD).