Skip to main content
. 2016 Sep;106:228–232. doi: 10.1016/j.carbon.2016.05.032

Fig. 1.

Fig. 1

a. Photographs of NRL and rGO/NRL composite films after dip molding on glass mandrels. b. Photographs of wPU and rGO/wPU composites at different rGO loadings after release from their glass mandrels and c. NRL, GO/NRL and rGO/NRL ring tensile test specimens obtained from (a). (A colour version of this figure can be viewed online.)