Changes in the physical characteristics of 10-HCPT nanocrystals after lyophilization

Process Size (nm) Polydispersity index Zeta potential (mV)
Before lyophilization 133.5±0.3 0.13±0.02 −27.1±1.36
Reconstitution with glucose 137.6±2.1 0.14±0.01 −27.2±2.32

Notes: All values are presented as mean ± SD; n=3.

Abbreviation: SD, standard deviation.