Skip to main content
. 2016 Jun 28;4:52. doi: 10.3389/fbioe.2016.00052

Figure 3.

Figure 3

Comparison of stress-strain curves (A) and tensile modulus (B) of the two most suitable membranes 250 μm and 300 μm thick and the braid-core obtained by interlacing the 300 μm thick membrane. Samples had been previously hydrated. *p < 0.05, **p < 0.001.