Skip to main content
. 2016 Jun 17;2(6):e1501591. doi: 10.1126/sciadv.1501591

Fig. 4. Degradation of HDPE-2 (120 to 135 mg) with n-octane (4 ml) by 2 (4.2 μmol Ir) and Re2O7/γ-Al2O3 (57.0 μmol Re2O7) at 175 °C after 2, 4, 6, 8, 24, 48, and 96 hours.

Fig. 4

(A) Distributions (wt %) of oil and wax products. (B) Mw of the isolated PE wax products. (C) Molecular weight distributions (PDI) of the isolated PE wax products.