TABLE 1.
Characterization of SiNPs with (+) and without (−) FITC in the core
Data are from n = 5 independent measurements (at 25 °C, in DMEM (+10% FCS) at 37 °C) performed within the first hour after transfer into the corresponding medium. TRM, transmission electron microscopy; DLS, differential light scattering. Ø = diameter; ζ = zeta potential.
Nanoparticle type | Ethanol |
Water |
DMEM (+ 10% FCS) |
|||
---|---|---|---|---|---|---|
Ø/nm (TEM) | Ø/nm (DLS) | ζ/mV | Ø/nm (DLS) | ζ/mV | Ø/nm (DLS) | |
SiNPs (+FITC) | 75 ± 2 | 107 ± 1 | +51 ± 1 | 119 ± 2 | +25 ± 1 | 245 ± 4 |
SiNPs (−FITC) | 52 ± 2 | 105 ± 3 | +37 ± 7 | 118 ± 6 | +33 ± 2 | 150 ± 15 |