Skip to main content
. 2015 Mar;49(1):27–35. doi: 10.15644/asc49/1/4

Table 2. Comparison of translucency before and after corrosion among materials of the same colour; t0 = translucency before exposure to corrosive medium; t1 = translucency after exposure to corrosive medium.

        AS±SD         p*         η2
        Translucency t0         A2         IPS e.max Ceram Dentin         7.58±0.92a
        IPS e.max Press         16.50±0.33b
        IPS e.max CAD
        14.17±0.85c
        <0.001
        0.966
        C2         IPS e.max Ceram Dentin         8.61±0.34a
        IPS e.max Press         17.53±0.50b
        IPS e.max CAD
        13.87±1.17c
        <0.001
        0.963
        B3         IPS e.max Ceram Dentin         9.69±0.30a
        IPS e.max Press         17.58±0.58b
        IPS e.max CAD
        14.27±0.50c
        <0.001
        0.981
        Translucency t1         A2         IPS e.max Ceram Dentin         7.50±0.69a
        IPS e.max Press         16.18±0.30b
        IPS e.max CAD
        13.95±0.68c
        <0.001
        0.978
        C2         IPS e.max Ceram Dentin         8.62±0.41a
        IPS e.max Press         17.52±0.68b
        IPS e.max CAD
        13.87±1.33c
        <0.001
        0.949
        B3         IPS e.max Ceram Dentin         9.62±0.48a
        IPS e.max Press         17.47±0.62b
        IPS e.max CAD         13.75±0.36c         <0.001         0.979

*ANOVA and Student-Newman-Keuls post-hoc test. Types of materials which have different letters in the exponent have a statistically significant difference within the same colour.