Skip to main content
. 2016 Jul 22;5(1):1158. doi: 10.1186/s40064-016-2783-3

Table 1.

Vertically aligned carbon nanotubes (VACNT) membrane parameters used to calculate the permeability and enhancement factor

VACNTs density (tubes cm−2) CNT diameter (nm) Dynamic viscosity µ (Pa S) at 20 °C Pressure difference Δp (torr) Membrane thickness (µm)
5 × 109–1 × 1011 8 1.002 × 10−3 140 25