Skip to main content
. 2016 Jul 22;7:12264. doi: 10.1038/ncomms12264

Figure 1. PNR results of E+T-conditioned sample.

Figure 1

(a) Fitted PNR data, with R++ (R−−) identified by solid circles (open triangles), scaled by q4 and (b) spin asymmetry for the sample as-grown and after E+T conditioning. (c) Depth-dependent real and imaginary nuclear SLD (ρN and ρimag), and magnetic SLD (ρM) extracted from the PNR. In all panels black, red and blue lines identify the as-grown, +40 V conditioned, and +/−40 V conditioned samples, respectively. In c the solid and dashed lines identify ρN and ρM, respectively, and the green line identifies ρimag. Background colours in c represent (red) Pd, (purple) AlOx, (green) GdOx and (yellow) Co, respectively. In a and b the experimental data are shown as symbols, and the lines are fits corresponding to the depth profile shown in c. Error bars in a and b correspond to ±1s.d.; error bars for c are shown in Supplementary Fig. 2. Arrows in a and b identify the bulk ρN for Co (2.25 × 10−4 nm−2) and CoO (4.29 × 10−4 nm−2).