Table 1. Parameter values obtained by fitting the experimental data to Equation (1).

Samples T0(K) τ0(s) Ea/KB(K)  
Ni50Mn38Ga12 65.1 9.3 × 10−14 43.8 canonical spin glass
Ni50Mn38Ga11Sb1 90.3 8.7 × 10−12 72.5 canonical spin glass
Ni50Mn38Ga10Sb2 130.7 2.4 × 10−10 104.1 cluster spin glass
Ni50Mn38Ga9Sb3 140.4 5.3 × 10−9 158.4 cluster spin glass
Ni50Mn38Ga8Sb4 147.5 7.2 × 10−9 173.3 cluster spin glass
Ni50Mn38Ga7Sb5 151.9 2.1 × 10−8 191.7 cluster spin glass
Ni50Mn38Ga6Sb6 156.4 1.3 × 10−7 213.6 cluster spin glass