Skip to main content
. Author manuscript; available in PMC: 2016 Aug 6.
Published in final edited form as: J Dent Res. 2008 Jul;87(7):671–675. doi: 10.1177/154405910808700706

Fig. 3.

Fig. 3

Side view video frames of cementation radial cracks (R) initiation in glass plate on polycarbonate bilayers with (a) axial and (b) off-axis loading following P = 75 N for n = 514 and P = 86 N for n = 547, respectively. Post mortem cementation view optical micrographs of respective glass/polycarbonate bilayers subjected to (c) axial loading at P = 75 N for n = 514 and (d) off-axis loading at P = 86 N for n = 547.