Table 5.
Catalyst loading |
Catalytic test temperature (°C) | n-Butanol selectivity (%) | References | ||
---|---|---|---|---|---|
mg | wt% | ||||
Mg and Al mixed oxides | 300 | 500 | >20 | [50] | |
ZrO2-supported Cu | 500 | 300 | ≥10 | [52] | |
Ni/Al2O3 | 10–50 | 250 | 80 | [53] | |
Hydroxyapatite | 350–450 | 50 | [54] | ||
Na to ZrO2 | 1 | 340–400 | – | [55] | |
Ni/C-alumina | 3000–3500 | 250 | 62 | [56] | |
Co2+ + / Ca2+ hydroxyapatite |
1.35 | 120–240 | – | [57] | |
MgO | 500 | 450 | – | [44] |