Skip to main content
. 2016 Apr 12;4(3):127–136. doi: 10.1080/21663831.2016.1166403

Figure 6.

Figure 6.

Brittle to ductile transition in SPD-processed iron. (a) Intercrystalline fracture at −196°C. (b) Pure dimple fracture at 200°C. (c) Increase of fracture toughness with increasing temperature with gradual change from grain boundary to dimple fracture.