Skip to main content
. Author manuscript; available in PMC: 2017 Feb 8.
Published in final edited form as: Biomacromolecules. 2016 Jan 25;17(2):601–614. doi: 10.1021/acs.biomac.5b01541

Figure 2.

Figure 2

SEM images of the liposome-cross-linked hybrid hydrogels after critical point drying. The average diameter of the liposomes embedded in the gel is 105 ± 25 nm, as analyzed by ImageJ.