Skip to main content
. 2016 Aug 11;2016:2876916. doi: 10.1155/2016/2876916

Figure 2.

Figure 2

(a), (c) 3D and (b), (d) 2D surface roughness images of an (a), (b) air or (c), (d) air APPJ treated polystyrene plate, and (e) a comparison graph of the Ra value (n = 5).