Skip to main content
. 2016 Sep 15;326:717–725. doi: 10.1016/j.jpowsour.2016.04.131

Fig. 3.

Fig. 3

CV study of 200 nm (200-nsC) and 500 nm (500-nsC)-thick electrodes in the IL N1113TFSI. Voltammograms at 100 mV s−1 with currents normalized to electrode area (a) and volume (b); area (c) and volumetric (d) electrode capacitances at different scan rates.