Skip to main content
. 2016 Aug 30;6:32171. doi: 10.1038/srep32171

Figure 4.

Figure 4

SEM images of the morphology of the 0.16Ag-TiO2 samples: (a) As-deposited and (be) Annealed at 200, 400, 600 and 800 °C respectively. The arrows indicate silver particles.