Wavenumber (cm−1) Vibrational mode Phase assignment
878 P-O stretching mode of PO4 group Brushite
948 P-OH stretching mode of HPO42− TCP
960 P-O stretching mode of PO4 group OCP
970 P-O stretching mode of PO4 group TCP
985 P-O stretching mode of PO4 group Brushite
1010 P-O stretching mode of HPO42− OCP