Skip to main content
. 2016 Aug 12;16(8):1281. doi: 10.3390/s16081281

Figure 3.

Figure 3

Square wave voltammetry 10 ppm of TNT in air saturated phosphate buffered saline (PBS) buffer measured at a fabricated epitaxial graphene working electrode on SiC (red), with oxygen modification (90 mTorr) (blue) and with nitrogen modification 50 mTorr (brown). The green trace is the background signal without TNT. Frequency = 60 Hz and Amplitude = 25 mV.