Comparison of sequence distribution on ice recrystallization inhibition activity. PVA70-rand-PVP20 random copolymer from previous work24 (Mn = 4320, Đ = 1.33, PVA = 48 wt %). Cartoons for PVA (blue) and PVP (black) are intended as a guide to structure only. MLGS = mean largest grain size relative to a PBS control, expressed as %. Error bars represent the standard deviation from at least three measurements.