Table 1. Means and standard deviations of shear bond strength values after three recycling procedures with sandblast technique and laser .

Group Time of recycling Mean ± SD 95% Confidence interval
(Lower‒Upper)
Sandblast Pre-recycling 32.45 ± 2.01 28.1336.77
First 25.58 ± 3.22 18.6732.49
Second 26.34 ± 2.19 21.6231.05
Third 30.75 ± 1.96 26.5334.96
Laser Pre-recycling 35.42 ± 2.52 30.0140.83
First 24.86 ± 1.98 20.6029.11
Second 22.76 ± 1.78 18.9426.59
Third 22.76 ± 1.51 19.5126.02