Figure 5. Electrochemical performance of TiS2/t-Na2.9375PS3.9375Cl0.0625/Na all-solid-state full cell.

Figure 5

Charge-discharge profile of TiS2/t-Na2.9375PS3.9375Cl0.0625/Na full cell at room-temperature. Cell was cycled under constant current conditions with a current density of 0.149 mA cm−2 (C/10 rate) from 1.2 V to 2.4 V. The cell was able to routinely deliver 80 mAh g−1 over 10 cycles. Red and black lines in the charge-discharge profile denote charging and discharging, respectively. Similarly, red and black markers signify charge and discharge capacities, while the green circles mark the coulombic efficiency by cycle.