. 2016 Aug 3;8(33):21545–21554. doi: 10.1021/acsami.6b05727

Figure 5.

Figure 5

(a) XRD spectra of the materials resulting from degradation at 60 °C after 7 days in SBF (b) HRTEM image showing the polycrystalline nature of the degradation byproducts (inset is a DFT image). (c) HRTEM image with higher magnification of a degradation byproduct. (d) Precipitation of sulfates with barium sulfate to demonstrate their presence using (A) Na2(SO4) as control, (B) degraded byproducts from the CuS NPs under the presence of the barium sulfate, and (C) without barium sulfate. (e) Precipitation of copper(II) ions with sodium hydroxide to demonstrate their presence: (D) degraded byproducts from the CuS NPs without NaOH and (E) with NaOH.