Skip to main content
. 2016 Aug 2;4(34):5673–5682. doi: 10.1039/c6tb01336h

Fig. 6. Turbidimetry scans (absorbance at 700 nm) of (A) blends with different mass fraction of PNIPAM100 coated Au15 and Au40, (B) PNIPAM50@Au15 and PNIPAM100@Au40 mixture with different mass fraction in PBS solution. In all cases the total gold core concentration of the solutions was 0.029 mg mL–1.