Fig. 6.
Non-contact optical profile testing instrument images of wear scars at 200 rpm under 40 N for 30 min. a For base oil. b For base oil with 1.0 wt.% ultrathin WS2 nanosheet
Non-contact optical profile testing instrument images of wear scars at 200 rpm under 40 N for 30 min. a For base oil. b For base oil with 1.0 wt.% ultrathin WS2 nanosheet