Skip to main content
. 2016 Oct 4;6:34086. doi: 10.1038/srep34086

Figure 3. PL intensity.

Figure 3

PL intensity from the stratified (a,c) and single layer (b,d) structures for single/stratified layer-acceptor (red) and donor-single/stratified layer-acceptor (blue) samples. In the single layer structure the thickness of silver film and in the stratified samples the metal-spacer-metal thickness is 60 (c,d) and 90 nm (a,b). The excitation source is 405 nm. The stratified samples show the higher SP-NRET efficiency and absolute photoemission compared to the single layer structures.