. 2016 Sep 26;2016:7456046. doi: 10.1155/2016/7456046

Table 2.

Comparison of E-modulus mean values for the tested materials.

Material E-modulus [MPa]
Mean value ± SD
(1) StoneBite 167.19 ± 19.59(1)
(2) Registrado X-tra 107.38 ± 11.36(1)
(3) O-Bite 93.94 ± 13.32(2)
(4) Variotime Bite 83.59 ± 8.76(3)
(5) Futar D 64.85 ± 9.05(4)
(6) Colorbite D 57.38 ± 7.52(5)
(7) Genie Bite 55.47 ± 7.27(6)
(8) Occlufast Rock 48.41 ± 7.38(6)
(9) Regidur i 48.11 ± 10.47(6)
(10) Omni-Bite Plus 47.88 ± 12.07(6)
(11) Jet Blue Bite fast 43.34 ± 9.66(7)
(12) Memoreg 2 42.22 ± 6.87(7)
(13) Regofix transparent 6.53 ± 2.34(8)

(1) p < 0.05 in comparison to (5)–(13).

(2) p < 0.05 in comparison to (6)–(13).

(3) p < 0.05 in comparison to (7)–(13).

(4) p < 0.05 in comparison to (1), (2) and (11)–(13).

(5) p < 0.05 in comparison to (1)–(3) and (13).

(6) p < 0.05 in comparison to (1)–(4) and (13).

(7) p < 0.05 in comparison to (1)–(5).

(8) p < 0.05 in comparison to (1)–(10).