. 2016 Oct 11;6:34958. doi: 10.1038/srep34958

Figure 6.

Figure 6

EBSD patterns of studied materials (a) without compression and compressed at (b) 500 MPa, (c) 1500 MPa, (d) 2000 MPa and (e) 2500 MPa. Different phase has different colours (blue- retained austenite; red- α′ martensite and yellow- ε martensite).