Table 1. Spin–lattice relaxation rate (1/T1) of 1 mL γ-Fe2O3@Au aqueous solution with and without light irradiation.
1/T1 (s−1) | ||||||
---|---|---|---|---|---|---|
Iron concentration (mM) | 0.21 | 0.14 | 0.095 | 0.048 | 0.021 | 0.0021 |
Light OFF | 2.372 ± 0.071 | 1.631 ± 0.045 | 1.320 ± 0.027 | 1.003 ± 0.036 | 0.758 ± 0.014 | 0.444 ± 0.013 |
Light On | 2.651 ± 0.050 | 1.835 ± 0.051 | 1.447 ± 0.019 | 1.090 ± 0.020 | 0.734 ± 0.017 | 0.444 ± 0.014 |
P-value | 0.0016 | 0.0032 | 0.0005 | 0.0379 | 0.1693 | 0.4950 |
The data are presented as the mean ± SEM from 10 measurements. The P-value is based on single-trail paired t-test calculation.