. 2016 Oct 17;7:13148. doi: 10.1038/ncomms13148

Figure 2. Fragmentation of modified film.

Figure 2

SEM images of of Ni(OH)2 thin film overgrowths for indicated thicknesses of 60, 80 and 120 nm, before and after thermal annealing. A magnified SEM image for the structures after annealing is also shown for each thickness. All scale bars are 2 μm in the main images and 500 nm in the magnified images.