Skip to main content
. 2016 Apr 8;59(7):270–276. doi: 10.1002/jlcr.3392

Table 1.

Binding efficiency of 89Zr to CN produced from various weight distributions of chitosan polymer

CN 15 kDa LMW (50–190 kDa) MMW (190–310 kDa)
89Zr uptake (%) 73.8 ± 18.8 (n = 30) 72.8 ± 24.4 (n = 8) 90.3 ± 14.8 (n = 8)

Incubation was carried out in a thermo‐shaker at 1400 rpm at room temperature for 45 min.