Table 1.
% cis | Crystallinity [%] | E 0 [MPa] | ϵ max [a] [%] | ϵ break [%] | Tensile toughness[b] [MJ m −3] | UTS [MPa] |
---|---|---|---|---|---|---|
80 | 22.3 | 59.8±0.2 | – | 1495±66 | 289±45 | 54.3±6.5 |
79 | 22.9 | 56.5±6.4 | – | 1554±71 | 330±29 | 56.7±5.2 |
70 | 14.1 | 26.2±0.3 | – | 1874±94 | 292±58 | 43.5±6.5 |
53 | 0 | 3.1±0.1 | 346 | 2252±115 | 104±22 | 16.6±3.8 |
32 | 0 | 2.7±0.1 | 378 | 2970±137 | 35±3 | 2.8±0.4 |
[a] ϵ max estimated from the value of the Young's modulus at small deformations. [b] Network toughness is calculated at a strain rate of 2.34×10−2 s−1.