Characteristics of the biofilm on plasticized polyvinyl chloride

Column(s) Temp (°C) ATP concn (avg ± SD)
Day 112 profile
Day 165 profile
Biofilm (ng/cm2) Water (ng/liter) Ratio B/Wa TCC (no./cm2)b HPC (CFU/cm2)c TCC (no./cm2) CH (μg/cm2)d Fe (μg/cm2) Mn (μg/cm2) Cu (μg/cm2)
1 38 27 ± 7 4.9 ± 2.0 6.8 ± 2.2 7.0 × 108 3.0 × 108 7.2 × 108 118 40 1.5 32
2 38 24 ± 11 4.6 ± 2.5 4.7 ± 2.3 6.7 × 108 1.4 × 108 5.0 × 108 108 38 1.4 28
3 38–42 22 ± 8 6.5 ± 3.7 4.6 ± 2.0 9.4 × 108 2.2 × 108 6.4 × 108 60 21 0.7 15
4 38 25 ± 7 4.3 ± 1.6 7.5 ± 3.2 5.3 × 108 1.3 × 108 5.1 × 108 96 42 1.8 35
5 38–42 23 ± 5 4.3 ± 3.2 7.7 ± 3.1 1.3 × 109 2.2 × 108 1.3 × 109 84 19 0.6 17
6 38 22 ± 6 5.7 ± 2.7 5.0 ± 1.5 9.5 × 108 2.0 × 108 6.9 × 108 132 30 1.1 24
7 38–42 26 ± 8 6.7 ± 2.4 4.3 ± 1.3 1.2 × 109 4.1 × 108 1.7 × 109 148 17 0.3 15
8 38 29 ± 8 7.3 ± 1.9 4.0 ± 1.1 5.3 × 108 2.2 × 108 4.3 × 108 113 25 0.9 15
9 38–42 22 ± 9 5.8 ± 1.4 3.1 ± 4.4 9.4 × 108 1.3 × 108 3.6 × 108 22 8.9 0.4 7
All (avg ± SD) 38 25.4 ± 2.8 5.4 ± 1.2 5.6 ± 1.5 (6.8 ± 1.7) × 108 (2.0 ± 0.7) × 108 (5.7 ± 1.3) × 108 113 ± 13 35 ± 7.2 1.3 ± 0.35 27 ± 7.8
All (avg ± SD) 38–42 23.2 ± 1.8 5.8 ± 1.1 4.9 ± 2.0 (11 ± 1.8) × 108e (2.5 ± 1.2) × 108 (10 ± 6.1) × 108 79 ± 53 16.5 ± 5.3e 0.5 ± 0.2e 13.5 ± 4.4e
a

Ratio of concentrations in biofilm (B) and water (W) from day 92 to day 154.

b

TCC, total cell count.

c

HPC, heterotrophic plate count.

d

CH, carbohydrate.

e

Significantly different (P < 0.05) from concentrations in columns operated at 38°C.