Skip to main content
. 2016 Oct 10;13(10):997. doi: 10.3390/ijerph13100997

Figure 1.

Figure 1

X-ray diffractometer (XRD) patterns of the samples: (a) La3+ with different dopant amounts calcined at 500 °C; (b) 0.75% La/TiO2 at different calcined temperatures.