. 2016 Oct 31;6:36119. doi: 10.1038/srep36119

Table 2. Surface characterization parameters resulting from fitting the NR curves for the DC film measured in air, D2O and with the adsorbed HRP layer.

Sample Thickness (Å) SLD (10−6 Å−2) Volume fraction Roughness (Å)
DC/Air 90 5.5 NA 15
DC/D2O 280 7.1 33 (cellulose) 8
HRP 98 3.9 20 (HRP) 17